Specifies four methods for the determination: method A50 using a force of 10 N and a heating rate of 50 °C/h, method B50 using a force of 50 N and a heating rate of 50 °C/h, method A120 using a force of 10 N and a heating rate of 120 °C/h, method B120 using a force of 50 N and a heating rate of 120 °C/h. The principle is determining the temperature at which a standard indenter penetrates 1 mm into the surface. The methods are applicable only to thermoplastics, for which they give a measure of the temperature at which the thermoplastics start to soften rapidly.
Informaciones generales
-
Estado: RetiradaFecha de publicación: 1994-07Etapa: Retirada de la Norma Internacional [95.99]
-
Edición: 3Número de páginas: 5
-
Comité Técnico :ISO/TC 61/SC 2ICS :83.080.20
- RSS actualizaciones
Ciclo de vida
-
Anteriormente
RetiradaISO 306:1987
-
Ahora
-
Revisada por
RetiradaISO 306:2004